Wat would the best ideal temp be for applying resin, also wat timescale is there before the resin becomes unusable when aplying to wraps.
Thanks to all.
 

·
Registered
Joined
·
3,273 Posts
Hi ,

i would say 20/22 degree (celcius!) is ideal . Pot life depends on room temperature and resin but it must be about 20/30 minutes ; if it becomes thicker during work , i sometimes make it thinner with a hot air gun (...just to finish that one wrap!) , but not too long ... best is not mixing too much resin in one time .

Cheers , Gert
 